3303 Industrial Metal Silicon

3303 Industrial Metal Silicon

Industrial Metal Silicon 3303 is produced through the high-temperature reduction of quartz with carbon in electric arc furnaces, followed by refining and quality control processes.
Hantar pertanyaan
Description/kawalan
Parameter teknikal
3303 Industrial Metal Silicon Description

 

Industrial Metal Silicon 3303 is produced through the high-temperature reduction of quartz with carbon in electric arc furnaces, followed by refining and quality control processes. Once produced, silicon metal is carefully packaged in bulk bags or smaller containers to protect it from contamination. It is then transported via truck, rail, or ship, with measures in place to safeguard its integrity. Upon reaching its destination, silicon metal is stored in dry, ventilated warehouses to maintain its quality.

Industrial Metal Silicon 3303

 

3303 Industrial Metal Silicon Composition

 

Si-3303 99.3 0.3 0.3 0.03

 

Particle size: 10-100mm,10- 50mm, 0-3mm, 2- 6mm and 3-10mm,etc.

Note: we can process the 2202, 3303,  441, 553 and other silicon materials into silicon powder of different granularities according to your needs.

 

 

Industrial Metal Silicon 3303 factoryIndustrial Metal Silicon 3303 for sale

 

 

 

 

A: Usually, we can deliver the goods within 15-20 days after we receive the prepayment or L/C.

A: 3000MT/month&Shipped in 20 days after payment.

 

Cool tags: 3303 industrial metal silicon, China 3303 industrial metal silicon manufacturers, suppliers